Quote:
Originally Posted by TurboM
I just cut it open today and applied about 5oz of JB weld across all of the holes. Pretty sure I got them all but it was a bit hard to see all of the ones on the bottom half. Not really sure what to do about the packing material though. I guess the 3 options are:
- put it back in chambers 1 and 3, or
- put it in the center chamber
- throw it in the trash
Any thoughts?
I'm having a local welder close it up tomorrow afternoon as the JB weld needs about 24hrs to fully cure. Based on the pictures I sent him he's pretty convinced the canister is stainless steel.
|
Did you close up all of the holes in all of the chambers? Or just chamber 2?
Also, what material did the welder use to close up the opening?